‹ All demos
25 Oct 2026 · Materials & Climate

Which metal mixes can hydrogen turn straight into alloy?

Instead of mining, smelting and melting each metal separately, you could blend their oxides and let hydrogen pull the oxygen out, leaving a finished alloy and only water as exhaust. This study works out, for thousands of cobalt–chromium–iron–manganese–nickel blends, how dry the hydrogen has to be for the last scrap of oxide to disappear.

Albert Linda, Shiv Shankar & Dierk Raabe

Why it matters

Metal production causes about 40% of global industrial greenhouse gas emissions, and hydrogen can turn a blend of oxides straight into an alloy in one step while giving off water instead of CO₂. This study maps how dry that hydrogen must be across 3,526 cobalt–chromium–iron–manganese–nickel blends: cobalt–iron–nickel mixes reduce easily (a median H₂/H₂O ratio of about 0.16 at 1100 °C), while manganese- and chromium-bearing mixes need gas hundreds to thousands of times drier, so recipes can be screened before anyone fires up a furnace.

The paper

Designing sustainable high-entropy alloys directly from mixed oxides: A thermodynamic perspective

Albert Linda, Shiv Shankar & Dierk Raabe (Max Planck Institute for Sustainable Materials, Düsseldorf). arXiv:2610.30870 [cond-mat.mtrl-sci], submitted 22 Oct 2026. Read on arXiv · PDF · Data & code

In plain language: every metal oxide holds on to its oxygen with a certain strength. Hydrogen can take that oxygen away (making water) only if the gas “pulls” harder than the oxide “holds”. How hard the gas pulls depends on the temperature and on the ratio of hydrogen to water vapour, r = H₂/H₂O. Drier gas (bigger r) pulls harder. The catch is that water builds up right where the reaction happens, so very large ratios are hard to keep.

In a blend, the metals dissolve in each other and the oxides mix, so each one holds its oxygen differently than it would on its own. The authors used CALPHAD thermodynamic databases (Thermo-Calc with TCOX10) to find, for each blend and temperature from 500 to 1500 °C, the last oxide that has to be removed, and the minimum gas ratio rmin that removes it. Manganese and chromium make that last oxide much harder to remove. Cobalt, iron and nickel make it easier. These effects can change size, or even reverse, depending on what else is in the mix. They also show that a blend with fewer in-between steps is not always easier to finish.

Try it: the hydrogen operating window

The gas line and the iron-oxide (FeO) line use the paper’s Equations 3, 4 and 6 exactly. Each coloured line is the median last-oxide stability for one family of three-metal blends. It comes from the paper’s median driving forces at 700 °C and 1300 °C and is drawn straight between them, which is an approximation. The open circles are a check, back-calculated from the paper’s median rmin at 1100 °C. A blend is reducible when its line sits above the gas line, inside the shaded zone.

Gas oxygen-pull line ΔGHyDR (kJ per mol O₂)
Water vapour in the H₂/H₂O gas
Margin for plain iron oxide (FeO → Fe)
Blend families whose median blend is fully reduced

Ellingham-style diagram: who holds oxygen harder, the oxide or the gas?
H₂/H₂O gas at your rFeO → Fe (dashed)Fe–Mn–NiCr–Fe–MnCr–Fe–NiCo–Fe–MnCo–Fe–Ni (1100 °C point)shaded: reducible zone
Driest gas needed, rmin (Equation 7)
your rcolours as above · circles: paper’s 1100 °C medians
Median rmin at your temperature
Blend familyrmin (this demo)Paper, 1100 °CMax H₂O in a 5% H₂ feedAt your r

The H₂O column is 5% ÷ rmin, as in the paper (for example, 121 ppm for Fe–Mn–Ni at 1100 °C). These are equilibrium targets at the reacting surface, not inlet specifications.

Try it: specific recipes at 900 °C

The paper lists the last-oxide energy (boundary 1) of six example blends at 900 °C (Figure 6). The last three rows are derived from the Conclusions: an equal iron–nickel blend needs r ≈ 0.3, and adding 10 at.% chromium or manganese lowers its last-oxide energy by about 168 or 161 kJ/mol O₂. Each bar is the driving force ΔGrf at your gas ratio. Green bars to the right reduce completely, red bars to the left leave oxide behind.

fully reducedoxide remainsnumbers at the right: rmin for that blend

What the paper found

ResultValue
Blends computed (Co–Cr–Fe–Mn–Ni, at 21 temperatures from 500–1500 °C)3,526 compositions
Reference gas: r = 3 is the smallest ratio that reduces FeO across 700–1300 °Crmin,FeO ≈ 2.6 at 700 °C
Median rmin at 1100 °C: Co–Fe–Ni / Cr–Fe–Ni / Fe–Mn–Ni / Co–Fe–Mn / Cr–Fe–Mn0.155 / 356 / 413 / 1,405 / 2,529
Fe–Mn–Ni median rmin, 700 °C → 1300 °C7.16 × 10⁴ → 71.2
Median driving force at r = 3, 700 → 1300 °C: Fe–Mn–Ni / Cr–Fe–Mn / Cr–Fe–Ni / Co–Fe–Mn−163→−82 / −190→−134 / −157→−87 / −181→−115 kJ/mol O₂
Most common last oxide in Fe-bearing blends: rock-salt (HALITE) / CORUNDUM / SPINEL42.4% / 28.6% / 27.6%
Adding 10 at.% Cr or Mn to equal Fe–Ni at 900 °C−168 / −161 kJ/mol O₂; rmin 0.3 → above 10³
Adding 10 at.% Co to equal Fe–Ni at 900 °C< 1 kJ/mol O₂ change

Sources: Section 3.1, Table 1, Section 3.4 and Conclusions of arXiv:2610.30870. Everything is equilibrium thermodynamics. It says nothing about speed: pores that trap water, gas flow and diffusion decide how fast, and whether, reduction finishes in practice. The metal is assumed to form a single FCC solid solution, which is a modelling assumption.

The maths

Hydrogen burning to water sets the oxygen potential of the furnace gas (T in kelvin, J per mol O₂). At a gas ratio r = pH₂/pH₂O:

2H₂ + O₂ → 2H₂O: ΔG°H₂O(T) ≈ −483,600 + 88T ΔGHyDR(T, r) = ΔG°H₂O − 2RT ln r

The last oxide in a blend has an onset energy ΔGonset (kJ per mol O₂). The reduction driving force and the minimum gas ratio follow from Equations 5 and 7:

ΔGrf = ΔGonset − ΔGHyDR/1000 rmin = exp[(ΔG°H₂O(T) − 1000 ΔGonset) / (2RT)]

Reduction is complete at equilibrium when ΔGrf > 0, that is, when r > rmin. The iron-oxide reference is ΔGFeO ≈ (−544,000 + 134T)/1000 kJ/mol O₂. Because rmin is exponential, small energy differences matter a lot. At 1100 °C, ±10 kJ/mol O₂ changes rmin by a factor of about 1.55, as the paper notes.

Check: at 700 °C and r = 3 the demo gives a gas line of −415.7 and an FeO line of −413.6 kJ/mol O₂, a margin of +2.1, matching Table 1. Family lines: ΔGonset(T) = ΔGHyDR(T, 3)/1000 + median ΔGrf, taken at 700 and 1300 °C and joined with a straight line. At 1100 °C this lands within a few kJ/mol O₂ of the paper’s own median rmin values (the open circles). The gap is small but noticeable on a log scale. The Co–Fe–Ni family is shown only at 1100 °C, because the paper gives its median as a number only at that temperature.

How to use it

Demo by Grok Bot for the Daily Research Explorer. Calculations run in your browser. Every input number is quoted from arXiv:2610.30870. The straight-line family curves and the three derived Fe–Ni recipes are this demo’s approximations, as labelled above.